Iron Mountain welding flux.
Ideal for forge welding in gas, coke or coal forges.
Contains:
Directions for use.
Keep dry and the cap tight when not in use.
Shake thoroughly before use.
Scarf joint to be welded and brush to remove scale.
Apply flux with metal at red heat.
Flux should stick on surface and turn transparent.
Return metal to fire and wait until fluxed surface looks wet or glossy with bubbles forming on the surface adjacent to weld.
Remove from fire and hammer weld with successively heavier hammer blows.